MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance, and excellent electrical properties.

Features: Good Chemical Resistance; Good Color Stability; High Reflectivity; Light Stabilized; Low Moisture Absorption

Uses: LEDs

Injection Molding Notes: A general purpose screw is recommended, with minimum back pressure.

Additional Properties: Mold Shrinkage - 1.0 %; Mold Shrinkage - 0.55 %; Optical Reflectivity - ASTM E1331 > 90 %; Optical Reflectivity - ASTM E1331 > 90 %; Optical Reflectivity - ASTM E1331 > 90 %; Tensile Strain at Break - ASTM D638 0.95 %

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Filler Content 22 %22 %Mineral
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 95.1 MPa13800 psiASTM D638
Tensile Stress 102 MPa14800 psiISO 527-2
Elongation at Break 1.1 %1.1 %ISO 527-2
Tensile Modulus 10.9 GPa1580 ksiISO 527-2
 11.0 GPa1600 ksiASTM D638
Flexural Strength 145 MPa21000 psiISO 178
 168 MPa24400 psiASTM D790
Flexural Modulus 9.93 GPa1440 ksiISO 178
 10.2 GPa1480 ksiASTM D790
Izod Impact, Notched (ISO) 2.70 kJ/m²1.28 ft-lb/in²Type 1, Notch A; ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  21.0 µm/m-°C
@Temperature 150 - 200 °C
11.7 µin/in-°F
@Temperature 302 - 392 °F
4
 24.0 µm/m-°C
@Temperature 100 - 150 °C
13.3 µin/in-°F
@Temperature 212 - 302 °F
4
 26.0 µm/m-°C
@Temperature 50.0 - 100 °C
14.4 µin/in-°F
@Temperature 122 - 212 °F
4
 27.0 µm/m-°C
@Temperature 200 - 250 °C
15.0 µin/in-°F
@Temperature 392 - 482 °F
4
CTE, linear, Transverse to Flow  51.0 µm/m-°C
@Temperature 50.0 - 100 °C
28.3 µin/in-°F
@Temperature 122 - 212 °F
TMA; ASTM E831
 73.0 µm/m-°C
@Temperature 100 - 150 °C
40.6 µin/in-°F
@Temperature 212 - 302 °F
TMA; ASTM E831
 110 µm/m-°C
@Temperature 150 - 200 °C
61.1 µin/in-°F
@Temperature 302 - 392 °F
TMA; ASTM E831
 130 µm/m-°C
@Temperature 200 - 250 °C
72.2 µin/in-°F
@Temperature 392 - 482 °F
TMA; ASTM E831
Melting Point 327 °C621 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 280 °C536 °F
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 - 318 °C579 - 604 °F
Front Barrel Temperature 316 - 329 °C601 - 624 °F
Melt Temperature 321 - 343 °C610 - 649 °F
Mold Temperature 135 °C275 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content <= 0.045 %<= 0.045 %
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormPellets
Processing TechniqueInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
RTP Company RTP 4000 AFA-6145 V0 (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber - Flame Retardant

PSOL8Y6953 / 176684

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.