MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2040226D2 Curable Carbon Ink
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and abrasion resistance. It offers the advantage of a One-Pak cure system combined with the convenience of Ambient Temperature stability, which means they do not have to be stored in a freezer or refrigerator.

General Purpose Grade

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size <= 5.0 µmFineness of Grind
Viscosity 5200 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake Viscosity
Thickness 20.0 - 30.0 microns
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 150 ohmcured; 25 microns thick
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 60.0 min
@Temperature 90.0 °C
 
Descriptive Properties
Coverage cm2/g295200 mesh stainless steel screen
Printing Mesh counts/inch180 to 340stainless steel or polyester screens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WGEM023 / 75876

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.