LNP FARADEX MS003 compound is based on Polypropylene (PP) resin containing 15% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding. Features: EMI/RFI Shielding,Electrically Conductive Information provided by SABIC |