MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Adsyl 5 C 30 F ST Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade (Polyolefin)

Material Notes: Adsyl resins are propylene plus ethylene and butene based random copolymers and terpolymers with high comonomer ratios that deliver improved sealing properties. Grades of Adsyl resins can be used in all of the main film extrusion technologies, such as BOPP, Double Bubble, Cast and Blown Film. Adsyl grades are mainly used for skin layers in co-extruded or coated film structures to provide sealing functionality.

Adsyl 5 C 30 F ST is an advanced polyolefin, specially designed for use as a sealing or metalized layer in co-extruded film applications. This grade features a very low seal initiation temperature and excellent optics. It does not contain slip or anti-block additives. Applications: Barrier Film, Breathable Film, Clarity Film, Food Packaging Film, Lamination Film, Sealants, Shrink Film, Specialty Film, Stationery Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 15.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Tensile Strength at Yield, TD 14.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Break, MD 900 %
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Break, TD 900 %
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Elongation at Yield, MD 18 %
@Thickness 0.0500 mm
500 mm/min, cast film; ISO 527-3
Film Elongation at Yield, TD 16 %
@Thickness 0.0500 mm
500 mm/min, cast film; ISO 527-3
Secant Modulus, MD 0.260 GPa
@Thickness 0.0500 mm
23 mm/min, cast film; ISO 527-3
Secant Modulus, TD 0.240 GPa
@Thickness 0.0500 mm
23 mm/min, cast film; ISO 527-3
Film Tensile Strength at Break, MD 41.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Film Tensile Strength at Break, TD 41.0 MPa
@Thickness 0.0500 mm
500 mm/min, Cast Film; ISO 527-3
Heat Seal Strength Initiation Temperature 105 °CLYB method
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 61.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 107 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 0.20 %
@Thickness 0.0500 mm
ASTM D 1003
Gloss 91 %
@Thickness 0.0500 mm
45°; ASTM D 2457
 
Descriptive Properties
Processing MethodBOPP, Cast Film, Double Bubble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adsyl 7572 XCP Polyolefin
LyondellBasell Adsyl 6 C 30 F Polypropylene terpolymer
ExxonMobil Vistamaxx™ 3980FL Propylene-based Elastomer - High Purity, Low Gel
ExxonMobil Vistamaxx™ 3588FL Performance Polymer
LyondellBasell Adsyl™ 5 C 30 F Polyolefin

PEQT7034 / 218673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.