MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SCG Chemicals J6573XXX PVC compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: J6573XXX is PVC compound product with any color for using in Fitting application product. The formulation is designed for Fitting & Ball Valve which give good process ability and Gloss surface by Injection Process.

Applications: Fitting and Ball Valve.

Features: Fitting and Ball Valve.

Features: Good process ability. Good surface of product. Good heat stability.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 - 1.40 g/cc1.34 - 1.40 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Izod Impact, Notched >= 0.392 J/cm>= 0.735 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 - 64.0 °C136 - 147 °FASTM D648
 
Descriptive Properties
AppearancePellet
Heat Stability80 minTPC Method @ 180°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC825 / 278082

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.