System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Polyram PB302G50 Nylon 6, 50% Glass Fiber
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 50% Glass Fiber Filled
Material Notes:
50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 international
Information provided by Polyram Ram On Ind.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.55
g/cc
0.0560
lb/in³
DIN 53479
Water Absorption
4.8 %
4.8 %
DIN 53495
Moisture Absorption at Equilibrium
1.5 %
1.5 %
50%RH; DIN 53714
Linear Mold Shrinkage
0.0020
cm/cm
0.0020
in/in
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
124
124
ASTM-D785
Tensile Strength, Yield
150
MPa
21800
psi
ASTM-D638
Elongation at Break
3.0 %
3.0 %
ASTM-D638
Flexural Strength
320
MPa
46400
psi
ASTM D790
Flexural Modulus
14.0
GPa
2030
ksi
ASTM-D790
Izod Impact, Notched
1.70
J/cm
@Temperature 23.0 °C
3.18
ft-lb/in
@Temperature 73.4 °F
ASTM-D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
DIN 53482
Surface Resistance
1.00e+12
ohm
1.00e+12
ohm
DIN 53482
Dielectric Constant
3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength
80.0
kV/mm
2030
kV/in
VDE 0303/4
Thermal Properties
Metric
English
Comments
Melting Point
218
°C
424
°F
Maximum Service Temperature, Air
110
°C
230
°F
Continuous Use
200
°C
392
°F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi)
220
°C
428
°F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi)
215
°C
419
°F
DIN 53461
Flammability, UL94
HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0
Celanese Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6
RTP Company RTP PA6 50 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized
RTP Company RTP 209 A Nylon 6 (PA), Glass Fiber
PPOLYRA179 / 57441
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.