MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformation of this critical component in ZIRCAR furnace insulation systems. The ultra high purity aluminum oxide content and superior creep resistance of these hanger clips make them ideal for use as the principal support member in high temperature furnace roof insulation systems operating as high as 1830°C (3326°F).

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.98 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Tensile Strength 300 - 400 MPa
Modulus of Elasticity 380 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 2053 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 99.999 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Mateck Sapphire (Al2O3)
Schott Sapphire Optical Window
Mateck Sapphire Aluminium oxide Substrate, Al2O3
Sapphire Spelling Note

CZIR907 / 138549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.