MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ajedium™ Film - Veradel® PES 201 NT Polyethersulfone (PESU)
Categories: Polymer; Film; Thermoplastic; Polyethersulfone (PES)

Material Notes: PESU film, high heat, high strength, good electrical properties,

Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C).

Veradel® film is resistant to oxidation and hydrolysis and withstand prolonged exposure to high temperatures and repeated sterilization. Veradel® 201 NT polyethersulfone films are highly resistant to mineral acids, alkali and salt solutions. Their resistance to detergents and hydrocarbon oils is good, but they will be attacked by polar solvents such as ketones, chlorinated hydrocarbons, and aromatic hydrocarbons.

Electrical properties of Veradel® PES films are stable over a wide temperature range and after immersion in water or exposure to high humidity.

The film is transparent, a light amber color.

Applications: Appliance Components; Automotive Electronics; Batteries; Electrical Parts; Electrical/Electronic Applications; Food Service Applications

Features: Acid Resistant; Alkali Resistant; E-beam Sterilizable; Food Contact Acceptable; Good Sterilizability; Good Toughness; High Heat Resistance; High Strength; Hydrolysis Resistant; Oxidation Resistant; Radiation (Gamma) Resistant

Standard Thicknesses and Widths
- Widths are available from 22" (559 mm) to 56" (1422 mm).
- Products with widths <22 inches or >56 inches are available upon request.
- Tolerances for widths are +/- 4mm.
- For PES film, the standard thicknesses are 25 microns (1 mil) to 1016 microns (40 mil).

Surface Finishes
- Standard surface finish is P/M (polished / matte).
- Custom finishes of P/P (polished / polished) and M/M (matte / matte) are available.

Packaging
- Film is supplied in a roll form of high quality, cardboard core of 3" (76mm) or 6" (152mm).
- PVC cores are available upon request in 3" and 6" sizes.

Labeling
- Products are labeled to comply with national and international standards.
- Labels include product grade, unique batch number, roll length, roll width, product thickness, and net weight.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Thickness 50.0 micronsAs Tested
 50.0 micronsAs Tested
 125 micronsAs Tested
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 71.3 MPaASTM D882
Film Tensile Strength at Yield, TD 71.4 MPaASTM D882
Film Elongation at Break, MD 140 %ASTM D882
Film Elongation at Break, TD 140 %ASTM D882
Film Elongation at Yield, MD 7.7 %ASTM D882
Film Elongation at Yield, TD 7.5 %ASTM D882
Secant Modulus, MD 2.10 GPaASTM D882
Secant Modulus, TD 2.09 GPaASTM D882
Elmendorf Tear Strength MD 120 gASTM D1922
Dart Drop Test 630 gASTM D1709
Film Tensile Strength at Break, MD 66.3 MPaASTM D882
Film Tensile Strength at Break, TD 65.8 MPaASTM D882
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 180 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 220 °CUnannealed; ASTM D648
Oxygen Index 39 %ASTM D2863
 
Descriptive Properties
Area Factor142 ft²/lb/mil
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorAmber
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4010 / 279810

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.