NAXALOY 780GF11 is an 11% Glass filled Polyester Blend of Polycarbonate and Polybutylene Terephthalate. This material is available in black, natural, and custom colors and either UV or non-UV stable. It is typically used for automotive exterior applications.Information provided by MCR Polymers |