MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GY-FR-P10 Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: low-smoke covering foamed product and various thermosetting resin and thermoplastic resin

Applications:

  • low-smoke covering foamed product
  • various thermosetting resin and thermoplastic resin
  • low fragibility isocyanate foamed plastic
  • PIR/PUR soft membrane foamed plastic
  • Flame retardant for unsaturated polyester resin
  • Various PU application
  • Phenolic resin
  • PVC (polyvinyl chloride)
  • Unsaturated polyester resin
  • excellent adhesive
  • coating and elastomer
  • acetic cellulose, nitric acid cellulose, epoxy resin etc.
  • laminate roofing and spray paint
Advantages:
  • Excellent fire proof ability
  • Outstanding heat stability
  • Soluble in most common organic solvents
  • Outstanding polymer compatibility
  • Good hydrolytic stability
  • Low acidity
  • Can provide adding value to products

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.288 - 1.298 g/cc0.04653 - 0.04689 lb/inĀ³
Viscosity 65 - 72 cP65 - 72 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.050<= 0.050mg KOH/g
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 32.5 %32.5 %
Phosphorus, P 9.5 %9.5 %
 
Descriptive Properties
Appearanceliquid
ColorTransparent or light yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN133 / 266441

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.