MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sipchem EVA 2018 CO 18% Ethylene Vinyl Acetate copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product description: Sipchem EVA 2018 CO is an 18% ethylene vinyl acetate copolymer resin, designed for a variety of foam moulding application; manufactured by IPC, an affiliate of Sipchem in The Kingdom of Saudi Arabia using an Exxon-Mobil high-pressure tubular process. EVA 2018 CO exhibits low melting temperature, good processability and mechanical properties.

Applications: Foams, Shoe Soles, Injection Moulding, Profile Extrusion, Films and Compounds.

Additives: Thermal Stabilizer: 300 ppm; Antiblock: No; Slip: No

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ASTM D792
Vinyl Acetate Content 18 %18 %ASTM D5594
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7676ASTM D2240
Hardness, Shore D 3636ASTM D2240
Tensile Strength at Break 11.0 MPa1600 psiASTM D638
Tensile Strength, Yield 5.20 MPa754 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Elongation at Yield 260 %260 %ASTM D638
Flexural Modulus 0.0600 GPa8.70 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 87.0 °C189 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPCH014 / 285327

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.