MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wingate Alloys Tuf-Last XL UHMW, PE for Coal, Ore and Aggregate Applications
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Bridging and arching are common problems in silos, bins and storage bunkers. Tuf-Last XL is the solution for material flow problems.

Ultra high molecular weight polymer exclusively designed to solve material flow, avrasion and corrosion problems. Modified with a silicone additive and answers challenges of moving difficult materials from coal, sand, gravel and wood pulp at freezing temperatures. Reduces bridging, arching and freezing with low coefficient of friction and zero moisture absorption.
Ultra high molecular weight polymer exclusively designed to solve material flow, abrasion and corrosion problems.
Modified with a silicone additive and answers challenges of moving difficult materials from coal, sand, gravel and wood pulp at freezing temperatures.
Excellent abrasion resistance. Outlasts steel 6 to 1. Resistant to most acids, alkalis and solvents and will not rust.
Does not absorb moisture and has a low coefficient of friction.
Lightweight and easily machined. Weighs about 1/8 as much as steel. Can be cut and drilled with basic power tools and is formable. Welded easily with plastic welding techniques.
Wide range of fasteners available for different attachment conditions

Reduces Bridging, Ratholing and Freezing: The low coefficient of friction and zero moisture absorption of Tuf-Last XL gives this engineering polymer exceptional non-stick properties to help reduce build-up of coal.

Resists Wear and Abrasion: Actual field applications demonstrate that Tuf-Last XL provides 6-10 times longer wear-life than steel. This exceptional resistance to sliding abrasion is due to Tuf-Last XL’s extremely high molecular weight and modifying components incorporated by our Manufacturer.

Eliminates Corrosion: Sulfur and other impurities found in coal have no corrosive effects of Tuf-Last XL, which substantially increases lining life. Unlike steel, UHMW will not rust and will resist a wider range of chemicals than stainless steel.

Applications: In the coal and ore transportation field Tuf-Last XL can be used for dump truck linings, rail car, dragline buckets liner, shovel liner, front loader liner, scraper liner and conveyer liners. Coal preparation liners for chutes, hoppers and conveyer skirting and troughs. Excellent product for bulk handling grains, gravel, wood chips, gypsum, fly ash, dry cement, coal, chemical powders, fertilizers and sand.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Coal
Concrete, sintered pulverized-fuel ash aggregate
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Wingate Alloys Tuf-Last UHMW PE
Wingate Alloys Winco Poly NLT Engineered UHMW

PWINGA25 / 122089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.