MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek C86200 Med. Tensile Manganese Bronze
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: High strength and hardness copper-zinc alloy.

Applications: Steel mill nuts, ordnance parts, worm gears.

Information provided by MetalTek

Cast UNS C86200; Cast Grade C86200; Cast ASTM B271, B584, B148; Military MIL-C-15345-5; SAE 430A (Discontinued)

Key Words: Yellow Brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192192
Tensile Strength, Ultimate >= 620 MPa>= 89900 psi
Tensile Strength, Yield >= 310 MPa>= 45000 psi
Elongation at Break >= 18 %>= 18 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.0 %4.0 %
Copper, Cu 63 %63 %
Iron, Fe 3.0 %3.0 %
Manganese, Mn 3.0 %3.0 %
Zinc, Zn 27 %27 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek C86300 High Tensile Manganese Bronze
MetalTek C86500 Low Tensile Manganese Bronze
AISI Type 410S Stainless Steel
MetalTek C86400 Leaded Manganese Bronze
Ampco Metal AMPCO® 863 Manganese Bronze, Continuous Cast

NMETEK034 / 18284

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.