MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Toray PMC CFRT® TL-6000, MOD 1 Thermoplastic Composite Laminate
Categories: Polymer; Thermoplastic

Material Notes: Toray PMC CFRT® (TL-6000) is a reinforced thermoplastic composite that blends the benefits of a thermoplastic polymer matrix with woven carbon fibers for enhanced performance. Within the product range, 2 layer (MOD1, 2L), 3 layer (3L), or 4 layer (4L) products are available, all ultra-thin, lightweight, and resilient. This material can be drilled, ground, polished and adjusted after being formed with a heated gun. TL-6000 has a smooth high-gloss finish and transparent surface to show woven carbon fiber.

Features:

  • High strength and stiffness
  • High mechanical properties of “Thin & Light” (TL) laminates
  • Carbon fiber weave shown with a high-gloss and smooth finish
  • Choice of 2, 3, or 4 multilayers available
  • Core option available as MOD1 or with 4L
Product Type And Composition: CFRT® (Continuous Fiber Reinforced Thermoplastic) composite with carbon fiber and modified Polymethylmethacrylate (acrylic) resin

Typical Applications:

  • Orthosis knee and ankle bracing

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³
Thickness 2740 - 3200 microns108 - 126 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 266 MPa
@Thickness 3.02 mm
38600 psi
@Thickness 0.119 in
Flexural Modulus 29.0 GPa
@Thickness 3.02 mm
4210 ksi
@Thickness 0.119 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 195 - 200 °C383 - 392 °FForming
 
Descriptive Properties
ColorsNatural (Carbon)
Flexural Rigidity6700 N-cm3.02 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY8069 / 265467

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.