MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning Gorilla® Glass Victus® 2 Display Glass
Categories: Ceramic; Glass; Optical

Material Notes: Improved drop performance, up to 1m on 80-grit and up to 2m on 180-grit. High resistance to scratch and sharp contact damage. High retained strength after use. Superior surface quality, with the same advantaged scratch resistance as Corning® Gorilla® Glass Victus®Use includes protective cover material for the front and back of all electronic devices:
  • Smartphones
  • Notebook PCs
  • Tablets
  • Smartwatches and wearables
  • Smart Home devices
  • Cameras
  • Commercial and Point of Sale Displays

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.41 g/cc0.0871 lb/in³
Thickness 400 - 1200 microns15.7 - 47.2 milothers upon request
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 595595kg(f)/mm² (200 g load), Unstrengthened
 670670kg(f)/mm² (200 g load) Strengthened
Modulus of Elasticity 79.0 GPa11500 ksi
Poissons Ratio 0.220.22
Fracture Toughness 0.820 MPa-m½0.746 ksi-in½
Shear Modulus 32.2 GPa4670 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  6.33
@Frequency 2.986e+9 Hz
6.33
@Frequency 2.986e+9 Hz
 6.34
@Frequency 2.466e+9 Hz
6.34
@Frequency 2.466e+9 Hz
 6.36
@Frequency 1.977e+9 Hz
6.36
@Frequency 1.977e+9 Hz
 6.37
@Frequency 1.499e+9 Hz
6.37
@Frequency 1.499e+9 Hz
 6.37
@Frequency 5.99e+8 Hz
6.37
@Frequency 5.99e+8 Hz
 6.38
@Frequency 3.81e+8 Hz
6.38
@Frequency 3.81e+8 Hz
 6.38
@Frequency 4.90e+8 Hz
6.38
@Frequency 4.90e+8 Hz
 6.39
@Frequency 9.12e+8 Hz
6.39
@Frequency 9.12e+8 Hz
 6.4
@Frequency 2.72e+8 Hz
6.4
@Frequency 2.72e+8 Hz
 6.41
@Frequency 1.63e+8 Hz
6.41
@Frequency 1.63e+8 Hz
 6.45
@Frequency 5.40e+7 Hz
6.45
@Frequency 5.40e+7 Hz
Dissipation Factor  0.0080
@Frequency 5.40e+7 Hz
0.0080
@Frequency 5.40e+7 Hz
 0.0080
@Frequency 1.63e+8 Hz
0.0080
@Frequency 1.63e+8 Hz
 0.0080
@Frequency 4.90e+8 Hz
0.0080
@Frequency 4.90e+8 Hz
 0.0090
@Frequency 5.99e+8 Hz
0.0090
@Frequency 5.99e+8 Hz
 0.0090
@Frequency 2.72e+8 Hz
0.0090
@Frequency 2.72e+8 Hz
 0.0090
@Frequency 3.81e+8 Hz
0.0090
@Frequency 3.81e+8 Hz
 0.010
@Frequency 9.12e+8 Hz
0.010
@Frequency 9.12e+8 Hz
 0.010
@Frequency 1.499e+9 Hz
0.010
@Frequency 1.499e+9 Hz
 0.011
@Frequency 1.977e+9 Hz
0.011
@Frequency 1.977e+9 Hz
 0.011
@Frequency 2.466e+9 Hz
0.011
@Frequency 2.466e+9 Hz
 0.012
@Frequency 2.986e+9 Hz
0.012
@Frequency 2.986e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.88 µm/m-°C
@Temperature 0.000 - 300 °C
3.27 µin/in-°F
@Temperature 32.0 - 572 °F
Softening Point 878.0 °C1612 °F107.6 Poise
Annealing Point 631 °C1170 °F1013.2 Poise
Strain Point 579 °C1070 °F1014.7 Poise
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.51
@Wavelength 590 nm
1.51
@Wavelength 590 nm
Core
 1.52
@Wavelength 590 nm
1.52
@Wavelength 590 nm
Compression Layer
Transmission, Visible >= 90.5 %
@Wavelength 380 - 2000 nm,
Thickness 0.700 mm
>= 90.5 %
@Wavelength 380 - 2000 nm,
Thickness 0.0276 in
IR Transmittance >= 90.5 %
@Wavelength 380 - 2000 nm,
Thickness 0.700 mm
>= 90.5 %
@Wavelength 380 - 2000 nm,
Thickness 0.0276 in
 
Descriptive Properties
Photo-elastic Constant30.8 nm/cm/MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCORNG14i / 305729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.