MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILCOLAPSE® 710 Silicone Antifoam Compound
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® 710 is a 100% active silicone antifoam designed for use in aqueous and anhydrous media with emphasis on use in food-related applications. Effective even in somewhat alkaline conditions, SILCOLAPSE® 710 can be formulated into custom emulsions or used directly in defoaming non-aqueous media. It can be used for indirect food use according the FDA CFRs indicated herein.

Applications:

  • Detergents/Soaps - liquids, shampoos, and powdered formulations
  • Fermentation Processes
  • Food Related and Food Additives – processing seafood, potato chips, freeze-dried products, edible oils, material/products for indirect food contact, rendering
  • Formulated Antifoam Emulsions
  • Crop Protection – product formulations; emulsifiable concentrates and aqueous dispersions
Features:
  • Easy to use, either as is or pre-diluted
  • Cost efficient, effective at low doses
  • Chemically inert, will generally not alter the properties of the foaming medium
  • Effective at high temperatures

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature <= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Appearancetranslucent, opalescent/white, homogeneous liquid
Content100% Active
DiluentsHydrocarbon solvents

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP™ F574 Highly Conformable, Thermally Conductive Gap Filler

PBLUST009 / 190985

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.