MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray TOYOLAC™ ABS Resin 884-X01 ABS Polymer, Flame retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame retardant, V-0, 5VA, ABS-FR(17).

General Toyolac™ Notes: TOYOLAC™ ABS is a versatile thermoplastic consisting of acrylonitrile, butadiene, and styrene and it has unique set of properties combining strength, lightness, and aesthetics. TOYOLAC™ is widely used in both industrial and household goods due to its excellent mechanical, chemical, electrical properties, and superior processability.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in23°C/50% RH; Toray Method
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R  104
@Temperature 23.0 °C
104
@Temperature 73.4 °F
50% RH; ASTM D785
 104
@Temperature 23.0 °C
104
@Temperature 73.4 °F
ISO 2039-2
Tensile Strength 45.0 MPa6530 psiASTM D638
 47.0 MPa
@Temperature 23.0 °C
6820 psi
@Temperature 73.4 °F
ISO 527-1,2
Elongation at Break 5.0 %5.0 %ASTM D638
 5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
ISO 527-1,2
Flexural Strength 68.0 MPa9860 psiASTM D790
 74.0 MPa
@Temperature 23.0 °C
10700 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 2.31 GPa335 ksiASTM D790
 2.35 GPa
@Temperature 23.0 °C
341 ksi
@Temperature 73.4 °F
50% RH; ISO 178
Izod Impact, Notched 1.57 J/cm
@Thickness 12.7 mm,
Temperature 23.0 °C
2.94 ft-lb/in
@Thickness 0.500 in,
Temperature 73.4 °F
V-notched; ASTM D256
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
V-Notched; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FISO 75-1,2
 76.0 °C169 °FUnannealed; ASTM D648
Vicat Softening Point 80.0 °C176 °F
Flammability, UL94 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY9227 / 248916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.