MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Pearlstick™ 5778 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5778 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU).

Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability under accelerated test conditions as well as outstanding pigment dispersion characteristics. Because of its medium Tg, it offers excellent adhesion and easier calendaring for high quality video and audio formulations. An excellent video tape can be formulated by blending with other harder dispersing resins. It is also used for dispersing high-surface–area pigments as a polymeric dispersant.

Uses: Tape binder, inks, lacquers and polymeric dispersing polymer for pigment dispersion

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Brookfield Viscosity 60 - 70 cP15% T.S. in MEK, RVT Spindle #2, 20 RPM, 23°C
 70 - 80 cP15% T.S. in THF, RVT Spindle #2, 20 RPM, 23°C
 180 - 200 cP15% T.S. in Cyclohexanone, RVT Spindle #2, 20 RPM, 23°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78
Tensile Strength 34.5 MPaASTM D-412/D-638
Elongation at Break 250 %ASTM D-412/D-638
100% Modulus 17.9 MPa
@Strain 100 %
ASTM D-412/D-638
Peel Strength 0.100 kN/mT-peel, Mylar film, Cast in MEK; ASTM D-1876-72
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 38.0 °CASTM D-1525
Glass Transition Temp, Tg 31.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR5015 / 238885

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.