MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ascend Performance Materials Starflam® M10004 Polypropylene PP FR
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Starflam M10004 is an unfilled halogen free flame retardant PP for injection molded applications (also known as Starflam M1000Z240C).

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³DAM; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiDAM; ISO 527-2
Elongation at Break >= 50 %>= 50 %DAM; ISO 527-2
Tensile Modulus 1.50 GPa218 ksiDAM; ISO 527-2
Flexural Strength 28.0 MPa4060 psiDAM; ISO 178
Flexural Modulus 1.30 GPa189 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  2.50 kJ/m²
@Temperature -30.0 °C
1.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO)  13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1U
 60.0 kJ/m²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FUnannealed; DAM; ISO 75-2/A
Glow Wire Flammability Index 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 190 °C356 - 374 °FInjection
Middle Barrel Temperature 190 - 200 °C374 - 392 °FInjection
Front Barrel Temperature 190 - 200 °C374 - 392 °FInjection
Melt Temperature 190 - 200 °C374 - 392 °FInjection
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °FInjection
Drying Temperature 70.0 °C158 °FInjection
Dry Time 3.00 hour3.00 hourInjection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
Agency RatingsISO, 1043 PP FR(40)
AppearanceNatural Color
FeaturesChemical Resistant
 Flame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8702 / 293363

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.