MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Aquivion® P98 Perfluorosulfonyl Fluoride (PFSF), Pellets
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Pellets, sulfonyl fluoride form, EW 980 g/eq

Aquivion® P98 are perfluorinated pellets in the sulfonyl fluoride (-SO2F) form that exhibit an Equivalent Weight (EW) of 980 g/eq. This material is based on the unique Short Side Chain copolymer of Tetrafluoroethylene (TFE) and Sulfonyl Fluoride Vinyl Ether (SFVE) F2C=CF-O-CF2CF2-SO2F produced by Solvay.

Aquivion® P98 resin can be easily melt extruded into a variety of shapes. The extruder should be equipped with a standard three-zone metering screw devoid of barrier or mixing elements. Optimum temperature settings will depend on the configuration of the equipment, but generally range from 200 to 300°C.

Optionally, functional groups in the molded part are then hydrolyzed in baths or wet benches with a heated base (NaOH, KOH etc.) reaction which may take minutes or hours, depending on thickness and conditions.

Aquivion® P98 can be directly hydrolyzed as described, either completely or only on their outer surface. This will enable functional activity of the sulfonic acid / sulfonyl salt groups for ion-exchange operations or as an acid catalyst.

Like other fluoropolymers, Aquivion PFSA pellets are corrosive in the melt; therefore, all parts having prolonged contact with the melt should be made with corrosion-resistant materials such as Hastelloy®, Inconel®, Monel® or Xaloy®. Chrome or nickel plating is not recommended since they are typically only sufficient for brief processing tests. Aquivion® pellets are not harmful if used and handled according to standard processing procedures (see for example "The Guide to the Safe Handling of Fluoropolymer Resins" issued by the Society of the Plastics Industry). If handled inappropriately, pellets may release harmful toxic chemicals.

PACKAGING, SHIPMENT AND STORAGE
- Aquivion® pellets are delivered in standard polypropylene bottles and drums. Products should be kept closed in their original packaging.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.08 g/cc0.0751 lb/in³
Melt Flow  5.0 - 20 g/10 min
@Load 2.16 kg,
Temperature 270 °C
5.0 - 20 g/10 min
@Load 4.76 lb,
Temperature 518 °F
ASTM D1238
 10 - 50 g/10 min
@Load 5.00 kg,
Temperature 280 °C
10 - 50 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 8.00 - 10.0 J/g3.44 - 4.30 BTU/lbASTM D3418
Melting Point 230 - 250 °C446 - 482 °F
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorTranslucent
Equivalent Weight (EW) g/eq940 to 1020
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4140 / 279940

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.