MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Toagosei America Aron Alpha® Industrial Krazy Glue™ 803 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.

High gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous substrates. Military Spec MIL-A-46050C Class 3. A primer is required for hard-to-bond materials such as polyethylene, polypropylene, acetal, PET, nylon, soft PVC, silicone rubber, and glass.

General information about the Aron Alpha® product line: Cyanoacrylates are single component instant adhesives that bond a wide variety of surfaces with a strong, durable bond. They offer ease of application, a wide range of performance parameters, and reliable solvent-free bonding.

Toagosei Co., Ltd. produces cyanoacrylates in Japan, marketed as Aron Alpha® in Japan, Cyanolit® in Europe, and Krazy Glue® in the US. Elmer's Products markets Krazy Glue® to the retail trade and Aron Alpha® to the industrial trade in North America. Information provided by Elmer's Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 1500 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3300 psivs. polycarbonate; 60 s set time
 3800 psivs. aluminum; 30 s set time
 4400 psivs. steel; 30 s set time
 4600 psivs. rigid PVC; 15 s set time
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Manufacturer specifies clear but does not quantify thickness.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °Ctypically used at ambient temperature
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Cyanoacrylate Adhesive
Bamberger Polymers Bapolene® 4012F Polypropylene, Compounding/Extrusion Grade
Mitsubishi Chemical Advanced Materials Proteus™ Homopolymer PP White Polypropylene
Overview of materials for Epoxy Adhesive
Toagosei America Aron Alpha® Industrial Krazy Glue™ 101 Cyanoacrylate Adhesive

PARON29 / 24600

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.