MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Addocat® 106 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 106 is suitable for recipes which also contain 1,4 butanediol. Addocat 106 is specifically used for semi-rigid integral systems such as formulations for shoe soles, armrests for cars, etc. and for polyurethane coatings and elastomers manufactured by cold casting. Approximately 1 - 2 p.b.w. Addocat 106 to 100 p.b.w. polyol blend are used, depending on the demold time required. Demold time can be reduced even further by using organo-metallic compounds such as Addocat 201 (approx. 0.03 p.b.w.).

Function: Catalyst for polyurethane.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Water Absorption <= 0.50 %
Viscosity 110 cP
 
Thermal PropertiesOriginal ValueComments
Boiling Point 200 °CInitial
Pour Point -1.00 °F
Flash Point 111 °CASTM D93, DIN EN 22719
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearanceclear colorless to yellowish liquid
Specifications24.5-25.5%Active substance
 930 mg KOH/gOH-value

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fainplast Compounds PMP 001/14 Flexible PVC, Extrusion Modified with PU

PLANY8181 / 208574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.