Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Celanese Zytel® (PA66) 70G50HSLR BK509 PA66-GF50
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 50% Glass Fiber Filled
Material Notes:
50% Glass Reinforced, Heat Stabilized, Hydrolysis Resistant, Polyamide 66
Former DuPont product acquired by Celanese in 2022.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.57
g/cc
0.0567
lb/in³
DAM; ISO 1183
Moisture Absorption
1.30 %
@Thickness 2.00 mm
1.30 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number
150
cm³/g
1.50
dl/g
DAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow
0.0020
cm/cm
0.0020
in/in
DAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse
0.0080
cm/cm
0.0080
in/in
DAM; ISO 294-4, 2577
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
170
MPa
24700
psi
50% RH; ISO 527-1/-2
240
MPa
34800
psi
DAM; ISO 527-1/-2
Elongation at Break
2.8 %
2.8 %
DAM; ISO 527-1/-2
4.0 %
4.0 %
50% RH; ISO 527-1/-2
Tensile Modulus
13.0
GPa
1890
ksi
50% RH; ISO 527-1/-2
17.0
GPa
2470
ksi
DAM; ISO 527-1/-2
Poissons Ratio
0.33
0.33
50% RH
0.33
0.33
DAM
Charpy Impact Unnotched
9.00
J/cm²
@Temperature -30.0 °C
42.8
ft-lb/in²
@Temperature -22.0 °F
DS; 50% RH; ISO 179/1eU
9.50
J/cm²
@Temperature -30.0 °C
45.2
ft-lb/in²
@Temperature -22.0 °F
DS; DAM; ISO 179/1eU
9.50
J/cm²
@Temperature 23.0 °C
45.2
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
10.0
J/cm²
@Temperature 23.0 °C
47.6
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched
1.60
J/cm²
@Temperature 23.0 °C
7.61
ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
1.80
J/cm²
@Temperature 23.0 °C
8.57
ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
475
V
475
V
50% RH; IEC 60112
550
V
550
V
DAM; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
13.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
7.22
µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
17.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
9.44
µin/in-°F
@Temperature 73.4 - 131 °F
DAM; ASTM E 831
20.0
µm/m-°C
@Temperature 55.0 - 160 °C
11.1
µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow
44.0
µm/m-°C
@Temperature -40.0 - 23.0 °C
24.4
µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
Melting Point
261
°C
502
°F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)
255
°C
491
°F
DAM; ISO 75-1/-2
Glass Transition Temp, Tg
20.0
°C
68.0
°F
10°C/min; 50% RH; ISO 11357-1/-2
70.0
°C
158
°F
10°C/min; DAM; ISO 11357-1/-2
Flame Spread
<=
80.0
mm/min
@Thickness 1.00 mm
<=
3.15
in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Processing Properties
Metric
English
Comments
Melt Temperature
295
°C
563
°F
Optimum, Injection
285
-
305
°C
545
-
581
°F
Range, Injection
Mold Temperature
70.0
-
120
°C
158
-
248
°F
Injection
100
°C
212
°F
Optimum, Injection
Ejection Temperature
210
°C
410
°F
Injection
Drying Temperature
80.0
°C
176
°F
Injection
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Injection, Dehumidified Dryer
Moisture Content
<= 0.20 %
<= 0.20 %
Injection
Hold Pressure
50.0
-
100
MPa
7250
-
14500
psi
Range, Injection
Descriptive Properties
Drying Recommended
yes
Injection
FMVSS Class
B
ISO 3795 (FMVSS 302)
ISO designation
ISO 16396-PA66,GF50,M1CGHW,S14-160
Max. screw tangential speed (m/s)
0.2
Injection
Part Marking Code
>PA66-GF50<
ISO 11469
Polymer
PA66-GF50
Processing Hold Pressure Time (s/mm)
3
Injection
Resin Identification
PA66-GF50
ISO 1043
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDSX5343c / 254528
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.