MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 101 Mobilgrease EAL
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Mobilgrease EAL 101 and 102 are supreme performance greases designed specifically for applications which are environmentally sensitive. These products are biodegradable and virtually non-toxic greases formulated from a synthetic ester base fluid and a lithium soap thickener. The wax-free nature of the synthetic base fluid, together with its low traction coefficient, provide excellent low temperature pumpability and very low starting and running torque - a significant benefit considering many environmentally sensitive applications are located outdoors. Mobilgrease EAL 101and 102 were formulated for multipurpose outdoor applications where grease leakage or run out could contaminate soil, groundwater or surface water systems. They can be used for indoor applications where grease leakage could enter plant water systems. They are recommended for plain and rolling element bearings and couplings that operate at temperatures from -30ºC to 120ºC. Mobilgrease EAL 101and 102 are NLGI grade 1 and 2 respectively; both have ISO VG 100 base oils. Extensive field evaluation and commercial experience with these products around the world has confirmed good performance in a variety of applications ranging from marble quarry chain saws to hydro-turbines. Even though they are designed for environmental benefits, Mobilgrease EAL 101 and 102 stand up to very demanding performance standards and help extend equipment life and keep equipment running reliably and efficiently.

Mobilgrease EAL 101and 102 are two members of a family of Mobil Environmental Awareness Lubricants (EAL) specifically designed for applications where contamination of the environment is a risk. Mobilgrease EAL 101 (NLGI Grade 1) and 102 (NLGI Grade 2) are multipurpose greases formulated with an ISO VG 100 base fluid. They are designed for the lubrication of equipment in environmentally sensitive areas, including: Marine equipment; Water treatment plants; Dams, locks and water ways; Construction equipment; Farm machinery

Key Words: NLGI Grade 1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Kinematic Viscosity at 40°C (104°F) 100 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 300 kgASTM D2596
Four Ball Wear 0.500 mmASTM D2266
Penetration 325Worked, 25°C; ASTM D217
Timken Test 45.0 lb
 
Thermal PropertiesOriginal ValueComments
Dropping Point 182 °CASTM D2265
 
Descriptive Properties
Biodegradability Shake-Flake Test78OECD 301B, CO2 Evolution
Coloramber
Copper Strip Corrosion, ASTM D1301B24 hrs @ 150°C
Corrosion Prevention, ASTM D1743pass
Emcor/SKF Water Wash Test, IP 2200
Soap/Thickener Typelithium hyrdroxystearate
Water Washout, ASTM D1264, wt%15@ 79°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Mobil Vaculine 533
ExxonMobil 7 Mobilith SHC Series
ExxonMobil 2 Mobilux EP
ExxonMobil 100 Mobil DTE FM Series
ExxonMobil 0 Mobilux EP

WEXXON395 / 75820

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.