MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.

Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cable jacketing and profile extrusion.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84 - 90
@Time 5.00 sec
ASTM D2240
Tensile Strength 51.7 MPaASTM D412
 38.78 MPa
@Temperature 75.0 °C,
Time 4.838e+6 sec
30 mil sheet, Immersion in Water
 43.95 MPa
@Temperature 75.0 °C,
Time 2.42e+6 sec
30 mil sheet, Immersion in Water
 44.98 MPa
@Temperature 75.0 °C,
Time 1.21e+6 sec
30 mil sheet, Immersion in Water
 45.5 MPa
@Temperature 75.0 °C,
Time 605000 sec
30 mil sheet, Immersion in Water
 51.7 MPa
@Temperature 75.0 °C,
Time 0.000 sec
30 mil sheet, Immersion in Water
Elongation at Break 500 %ASTM D412
100% Modulus 0.00690 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0124 GPa
@Strain 300 %
ASTM D412
Tear Strength 150 pliTrouser; ASTM D470
Graves Tear Strength 500 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40H18, 1000g; ASTM D3389 B
Tensile Set 18 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 °CDSC
 150 °CKolfer
Glass Transition Temp, Tg -45.0 °CDSC
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %pressed between glass; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Zone 1 177 °CExtrusion
Zone 2 182 °CExtrusion
Zone 3 188 °CExtrusion
Zone 4 193 °CExtrusion
Adapter Temperature 193 °C5, Extrusion
Die Temperature 193 °C6, Zone 1, Extrusion
 193 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
 
Descriptive Properties
Volume swell in Water1.1%24h, 23°C; ASTM D471

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Nexeo® HIVAL® 500354 High Density Polyethylene
Covestro Texin® 985 Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 150 Thermoplastic Polyurethane
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane

PNOVEON058 / 55325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.