MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trinseo Magnum™ 2642 ABS, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The 2600 series of MAGNUM ABS resins are designated for use in healthcare applications. Both high and low gloss resins are available which have passed the USP XXIII Class IV medical testing. Other non-USP classified testing is also done on the MAGNUM 2600 series of ABS resins to evaluate the biocompatibility of the resins.

MAGNUM 2642 ABS resin is a low gloss ABS with impact resistance and processability similar to the high gloss MAGNUM 2610 ABS resin. With a melt flow rate of 6 g/10 min. and an Izod impact strength of 160 J/m, MAGNUM 2642 is suitable for many healthcare applications.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
Melt Flow 6.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104
Tensile Strength, Yield 41.4 MPaASTM Data
Elongation at Yield 2.1 %ISO Data
Tensile Modulus 1.79 GPaASTM Data
Izod Impact, Notched 1.60 J/cmASTM Data
Charpy Impact Unnotched 10.0 J/cm²ISO Data, Low Temp
 NBISO Data
Charpy Impact, Notched 0.700 J/cm²ISO Data, Low Temp
 1.30 J/cm²ISO Data
Instrumented Impact Total Energy 43.0 J
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 78.0 µm/m-°C
@Temperature 20.0 °C
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CUnannealed; ASTM Data
 96.1 °CAnnealed; ASTM Data
Vicat Softening Point 104 °C
 
Optical PropertiesOriginal ValueComments
Gloss 52.5 %Gardner Gloss, 60°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 1040 ABS, Very High impact
Trinseo Magnum™ 9010 ABS, High Gloss
Trinseo Magnum™ 2630 ABS, High Impact
Trinseo Magnum™ 2620 ABS, Impact Grade
Trinseo Magnum™ 213 ABS, General Purpose

PZZDW077 / 34308

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.