MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool CHROME
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kaowool Veneering modules, HP Grade, ZR Grade, *Saffil Grade are made from high-temperature grade Kaowool ceramic fibers or Saffil high alumina fibers. The modules are fabricated into 12" x 12" (305 mm x 305 mm) blocks using fiber strips turned edge-grain and slightly compressed with a gauze-type wrap. When the furnace is fired, the wrap will burn off and the modules will distend to provide a tight, uniform furnace lining.

Kaowool Veneering modules are part of the Unisystem family of products. They can be applied over a variety of refractory surfaces using K-Bond mortar. Unikote M or S surface coatings are normally applied over the module hot face to provide thermal stability and chemical attack resistance.

Features:

  • 12" x 12" (305 mm x 305 mm) blocks of ceramic fiber insulation
  • Easily installed over existing refractory surface
  • Improves furnace efficiency without replacing a serviceable refractory lining
  • Suitable for temperature ranges up to 3000°F (1649°C)
  • Excellent insulating properties
  • Applications:

  • Forge furnaces
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.128 g/cc0.00462 lb/in³Available in multiple densities
     0.160 g/cc0.00578 lb/in³Available in multiple densities
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0793 W/m-K
    @Temperature 260 °C
    0.550 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    10 pcf; ASTM C201
     0.0821 W/m-K
    @Temperature 260 °C
    0.570 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    8 pcf; ASTM C201
     0.143 W/m-K
    @Temperature 538 °C
    0.990 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    10 pcf; ASTM C201
     0.164 W/m-K
    @Temperature 538 °C
    1.14 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    8 pcf; ASTM C201
     0.239 W/m-K
    @Temperature 816 °C
    1.66 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    10 pcf; ASTM C201
     0.278 W/m-K
    @Temperature 816 °C
    1.93 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    8 pcf; ASTM C201
     0.353 W/m-K
    @Temperature 1090 °C
    2.45 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    10 pcf; ASTM C201
     0.406 W/m-K
    @Temperature 1090 °C
    2.82 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    8 pcf; ASTM C201
    Maximum Service Temperature, Air 1340 °C2450 °FContinuous
     1430 °C2600 °FRating
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 43 %43 %
    Cr2O3 3.0 %3.0 %
    SiO2 54 %54 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Chromium, Cr; As-Swaged
    Aluminum 384.0-F Die Casting Alloy
    Overview of materials for Chrome-moly Steel
    Sylvania SX195 Chrome Based Thermal Spray Powder
    Gold, Au

    CTHERM089 / 2409

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.