MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

White meranti (Shorea, Lauan-Meranti Group) Wood
Categories: Wood and Natural Products; Wood

Material Notes: Mechanical property data is based on clear, straight-grained specimens from Asia.

Key Words: lumber, timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.550 g/cc0.550 g/ccGreen, Asian Origin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4400 N989 lb (f)Side Hardness, Green, Asian Origin
 5100 N1150 lb (f)Side Hardness, 12% Moisture, Asian Origin
Modulus of Rupture 0.0676 GPa9.80 ksiStatic Bending, Green, Asian Origin
 0.0855 GPa12.4 ksiStatic Bending, 12% Moisture, Asian Origin
Flexural Modulus 9.00 GPa1310 ksiStatic Bending, Green, Asian Origin
 10.3 GPa1490 ksiStatic Bending, 12% Moisture, Asian Origin
Compressive Strength 37.9 MPa5500 psiParallel to Grain, Green, Asian Origin
 43.8 MPa6350 psiParallel to Grain, 12% Moisture, Asian Origin
Shear Strength 9.10 MPa1320 psiParallel to Grain, Green, Asian Origin
 10.6 MPa1540 psiParallel to Grain, 12% Moisture, Asian Origin
Work to Maximum Load 0.0560 J/cm³8.12 in-lb/in³Static Bending, Green, Asian Origin
 0.0700 J/cm³10.2 in-lb/in³Static Bending, 12% Moisture, Asian Origin
 
Thermal PropertiesMetricEnglishComments
Shrinkage 3.0 %3.0 %Radial Shrinkage Green to Oven Dry, Asian Origin
 6.6 %6.6 %Tangential Shrinkage Green to Oven Dry, Asian Origin
 7.7 %7.7 %Volumetric Shrinkage Green to Oven Dry, Asian Origin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSU145 / 282596

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.