MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Celstran® PP-GF40-02 PP, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: 40% long strand glass fiber reinforced polypropylene

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Density 1.21 g/cc0.0437 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 102 MPa14800 psi5mm/min; ISO 527-2/1A
 117 MPa17000 psiASTM D638
 72.4 MPa
@Temperature 93.3 °C
10500 psi
@Temperature 200 °F
ASTM D638
 176 MPa
@Temperature -40.0 °C
25500 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 1.9 %1.9 %ASTM D638
 2.1 %2.1 %5mm/min; ISO 527-2/1A
 1.8 %
@Temperature 4.44 °C
1.8 %
@Temperature 40.0 °F
ASTM D638
 2.43 %
@Temperature 93.3 °C
2.43 %
@Temperature 200 °F
ASTM D638
Tensile Modulus 7.70 GPa1120 ksi50mm/min; ISO 527-2/1A
 9.17 GPa1330 ksiASTM D638
 5.69 GPa
@Temperature 93.3 °C
825 ksi
@Temperature 200 °F
ASTM D638
 11.7 GPa
@Temperature -40.0 °C
1690 ksi
@Temperature -40.0 °F
ASTM D638
Flexural Strength 180 MPa26100 psiISO 178
 186 MPa27000 psiASTM D790
 99.3 MPa
@Temperature 93.3 °C
14400 psi
@Temperature 200 °F
ASTM D790
 294 MPa
@Temperature -40.0 °C
42600 psi
@Temperature -40.0 °F
ASTM D790
Flexural Modulus 7.65 GPa1110 ksiASTM D790
 8.06 GPa1170 ksiISO 178
 4.44 GPa
@Temperature 93.3 °C
644 ksi
@Temperature 200 °F
ASTM D790
 11.4 GPa
@Temperature -40.0 °C
1650 ksi
@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 2.72 J/cm5.10 ft-lb/inASTM D256
 3.58 J/cm
@Temperature -40.0 °C
6.70 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.84 J/cm
@Temperature 93.3 °C
7.20 ft-lb/in
@Temperature 200 °F
ASTM D256
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 152 °C305 °FASTM D648
 152 °C306 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 70.0 °C104 - 158 °Fcavity
Feed Temperature 20.0 - 50.0 °C68.0 - 122 °F
Zone 1 210 - 220 °C410 - 428 °F
Zone 2 220 - 230 °C428 - 446 °F
Zone 3 230 - 240 °C446 - 464 °F
Zone 4 230 - 250 °C446 - 482 °F
Die Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 230 - 250 °C446 - 482 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 hour2.00 hour
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF40-03-Black PP, 40% Glass Reinforced
Envalior Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry)
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Conditioned)
Celanese Celstran® PP-GF30-02 AD 3002 PP, 30% Glass Reinforced

PHCQ220 / 178675

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.