MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa DANADD® CL-02 Organic chlorine compound
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® CL-02 is a high quality chlorine donor to produce halogenation´s primers. DANADD® CL-02 is mainly needed by the production of 2component-halogenizers.

Application: DANADD® CL-02 is often packed in small units by the adhesive industry. By the packaging of DANADD® CL-02 it must be observed that only containers are suitable which are made of glass or plastic. The commonly used solvents for the halogenations dilutions are ethylene acetate and methylene chloride. For the most part the solvent will be offered as component (I) in a unique packaging size. The mixing of the halogenation’s dilution will take place just before the processing will start by the final customer. We recommend as halogenation formula: DANADD® CL-02 1,5 parts of weight Solvent (acc. as a.m.) 98,5 parts of weight 100,0 parts of weight Such produced halogenations primers can be stored at room temperature and in a dark place up to 10 days and it will still be suitable to be processed.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³DIN 51.757
Solids Content 100 %100 %DIN 53.189
Storage Temperature 0.000 - 25.0 °C32.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FKOFLER
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Aspectwhite granulates
Composition0.92Active chlorine content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ002 / 294422

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.