PA 6, film , medium viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide" Application Examples: flat and blown film, monofilaments, biaxially stretched films Former Lanxess product line is now with Envalior. |