MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.

Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry for engine components, such as water tanks, degassing and liquid containers, engine covers, and various housing.

This product is available in natural, black and in colors on request.

Glow wire test thick. 1,6 mm, IEC 695-2-1, is 700°C.

Information provided by Rhodia; Rhodia has been acquired by Solvay.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Key Words: Polyamide 66; PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccISO 1183-A
Water Absorption 0.80 %24 hours in water at 23°C; ISO 62.
Linear Mold Shrinkage 0.0050 cm/cmRHODIA-EP
Linear Mold Shrinkage, Transverse 0.0080 cm/cmRHODIA-EP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 190 MPaISO 527
Tensile Strength, Yield 190 MPaISO 527
Elongation at Break 3.0 %ISO 527
Tensile Modulus 10.0 GPaISO 527
Flexural Yield Strength 260 MPaISO 178
Flexural Modulus 8.40 GPaISO 178
Izod Impact Resistance 1.10 J/cm²ISO 180
Charpy Impact Unnotched 8.00 J/cm²ISO 179/EU-1993
Charpy Impact, Notched 1.20 J/cm²ISO 179/1EA-1993
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.00e+14 ohm-cmIEC 93
Surface Resistance 6.00e+14 ohmIEC 93
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 34.0 kV/mmIEC 243-1
Dissipation Factor 0.010
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 450 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ASTM E831
Melting Point 263 °CISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75-2
Flammability, UL94 HB
@Thickness 1.60 mm
ISO 1210/UL 94
Oxygen Index 23 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 270 °C
Middle Barrel Temperature 270 - 280 °C
Front Barrel Temperature 280 - 290 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH50
Domo Technyl® A218 Heat Stabilized Nylon 66
Solvay Engineered Polymers Dexflex® 480 TPO
Domo Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Domo Technyl® C216V30 30% Glass Filled Nylon 6

PRHO04 / 65935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.