System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Solvay Thornel® Mat VMD Carbon Fiber
(discontinued **)
Categories:
Carbon
;
Carbon Fiber/Carbon Fibre
;
Other Engineering Material
;
Composite Fibers
Material Notes:
Form of mat VMA with shorter fibers for injection molding. Fiber lengths average 400 µm - adequate for good property improvement.
98% carbon assay, 13 µm filament diameter
Solvay has acquired the Thornel product line as a part of the Cytec purchase.
Key Words:
Carbon Fibre
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
2.00
g/cc
0.0723
lb/in³
Filament Property.
Apparent Bulk Density
0.200
g/cc
0.00723
lb/in³
Specific Surface Area
0.40
m²/g
0.40
m²/g
Filament Property
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
1400
MPa
203000
psi
Filament Property. Mat strength is 120 N/m
Tensile Modulus
170
GPa
24700
ksi
Filament property
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00120
ohm-cm
0.00120
ohm-cm
Filament
0.700
ohm-cm
0.700
ohm-cm
Mat
Thermal Properties
Metric
English
Comments
Thermal Conductivity
0.410
W/m-K
2.85
BTU-in/hr-ft²-°F
across thickness of mat
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Solvay Thornel® Mat VME Carbon Fiber
Solvay Thornel® Mat VMC Carbon Fiber
Solvay Thornel® Mat VMA Carbon Fiber
Solvay THORNEL® P-25 Pitch-Based Fiber
Solvay THORNEL® P-30 Pitch-Based Fiber
ETHORO / 6096
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.