MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M EC-2 Cold Shrink End Caps
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the core is removed to provide a reliable environmental seal. Four different end caps are available to accommodate a wide range of sizes.

Applications: Moisture sealing a physical protection for cables, pipes or other cylindrical objects.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption 1.8 %1.8 %7 days @ 90°C
Thickness 16000 - 30000 microns630 - 1180 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 9.65 MPa1400 psiASTM D412-75
Elongation at Break 750 %750 %ASTM D412-75
300% Modulus 3.31 MPa
@Strain 300 %
480 psi
@Strain 300 %
ASTM D412-75
Tear Strength 26.3 kN/m150 pliDie C; ASTM D624C-73

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35118 / 169865

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.