MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF 2- Ethylhexyl Acrylate
Categories: Fluid

Material Notes: Formula: C11H20O2

CAS: 203-080-7

Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses.

Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. Copolymers of 2-ethylhexyl acrylate can be prepared with acrylic acid and its salts, amides and esters, and with methacrylates, acrylonitrile, maleic acid esters, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils, etc. 2-ethylhexyl acrylate is also a very useful feedstock for chemical syntheses, because it readily undergoes addition reactions with a wide variety of organic and inorganic compounds.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.887 g/cc0.0320 lb/in³
Viscosity 1.7 cP1.7 cP
Molecular Weight 184.3 g/mol184.3 g/mol
Vapor Pressure 1.00e-6 bar0.000750 torr
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.89 J/g-°C0.452 BTU/lb-°Fof Liquid
Melting Point -90.0 °C-130 °FFreezing Point
Boiling Point 91.0 °C196 °F13 mbar
 216 °C421 °F1013 mbar
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4351.435
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %ASTM D203
 
Descriptive Properties
Assay>99.6%
Color<10APHA, ASTM D1209
Heat of Polymerization332 kJ/kg
Latent Heat of Evaporation at Boiling Point248 kJ/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® HF-5330S ASA, Unreinforced
Arkema LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate
Arkema LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate
Arkema LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate

PBASG0961 / 132594

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.