Varcum 29319 is a long-flow, two-step, powdered phenolic resin, which is processed using standard coldpress techniques. APPLICATION: - Brittle, coolant resistant bond structures for use in such grinding applications as roll grinding, tool room grinding, specialty grinding and the cutting of ceramic materials.
- Wheels formulated with this resin provide and easy, fast, cool cutting action which is particularly effective in critical metal grinding applications where overheating or burning of the metal must be minimized.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |