MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alumina, alpha Al2O3, 99.5%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Property values below are taken from literature and manufacturer sources. Variations are possible among various commercial grades.

Key Words: aluminum oxide, corundum
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.90 g/cc
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Tensile Strength, Ultimate 260 MPa
Modulus of Elasticity 370 GPa
Flexural Strength 350 MPa
Compressive Strength 2600 MPa
Poissons Ratio 0.22
Fracture Toughness 4.00 MPa-m½
Shear Modulus 140 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cm
Dielectric Constant 9.7
Dielectric Strength 9.00 kV/mmWide Variation Between Grades
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.60 µm/m-°C
@Temperature 25.0 - 400 °C
 8.20 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.880 J/g-°C
Thermal Conductivity 30.0 W/m-K
 12.0 W/m-K
@Temperature 400 °C
 26.0 W/m-K
@Temperature 100 °C
Maximum Service Temperature, Air 1700 °CNo Load
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Overview - Alumina, 98%, Al2O3
Alumina, alpha Al2O3, 96%
Overview - Alumina, 96%, Al2O3
Corning Macor® Machinable Glass Ceramic

BA5A / 143

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.