MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Body Double™ Standard Set Silicone rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Body Double™ is a long lasting platinum-cure silicone rubber that can be applied directly to the skin to make molds of the face, hands and other body parts. The rubber cures quickly and will reproduce perfect detail from any original model – far better detail than any alginate! Body Double™ is skin safe and certified by an independent laboratory. One Casting or Many . . . For About The Same Price: unlike alginates, which are good for one only casting, Body Double™ will last for many castings of almost any material including plaster, Matrix™ Neo™, wax, resins (Smooth-Cast urethanes, polyester, etc.), lowtemperature melt metal alloys, etc. The amount of Body Double™ used per mold is less than most alginates, so the cost per mold is about the same. Adding HYPER-FOLIC™ release additive to Body Double™ silicone will create a self-releasing silicone which is easily removed from hair-covered body areas. Body Double™ “Fast Set” for fast turnaround. Working time of 90 seconds and a demold time of 7 minutes

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2525ASTM D-2240
Tensile Strength 3.62 MPa525 psiASTM D-412
Elongation at Break 500 %500 %ASTM D-412
Tear Strength 7.01 kN/m40.0 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min0.0833 hourWorking
 20.0 min0.333 hourDemold
Pot Life 5.00 min5.00 minASTM D-2471
 
Descriptive Properties
ColorPurple
Mix Ratio1A:1Bby weight
Mixed ViscosityBrushable
Specific Volume23.7[in3/lb], ASTM D1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN314 / 297015

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.