MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Akrochem Superpoly 50 Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Description: The Superpoly (SP) line of specialty polyisoprene natural rubbers is partially pre-crosslinked, high performance elastomers available in bale form. These elastomers are produced by blending specific proportions of vulcanized and unvulcanized natural rubber during the latex phase of production. The latex phase blending ensures a homogeneous, uniform mix of the two components. Due to their unique two-phase structure, SP natural rubbers are very clean, light in color and contain low levels of volatile matter.

Applications: Superpoly natural rubbers are used in quality formulations as either the sole elastomer or as a blend (process aid) with other natural or synthetic elastomers. These natural rubbers have the ability to improve flow characteristics and increase mix viscosities which are advantageous properties to mixing, preforming and molding rubber. For extruded goods, SPs create fast throughput, low die swell, smooth surfaces and increase dimensional stability. Applications include: wiper blades, tubing, hoses, sponge, surgical articles, gaskets, windscreen seals, etc. For calendered parts, SPs reduced shrinkage and improve surface finish and gauge consistency. Uses include: sheeting, tape, cut threads, railway pad ballast, etc. With the use of SPs, molded goods benefit with less air and volatile entrapment (blisters), gauge consistency, surface appearance, etc. SP-20S is a special grade used in solvent adhesive systems to develop body, resistance to cold flow, and high temperature resistance. This grade has the special ability to maintain a lower solution viscosity compared to a conventional natural rubber with the same mooney viscosity and concentration; thus, higher solids levels are possible with the same viscosity.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.32 %0.32 %
Mooney Viscosity 50
@Temperature 100 °C
50
@Temperature 212 °F
ML 1+4
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 0.49 %0.49 %
Sulfur, S 0.25 %0.25 %Free
 1.15 %1.15 %Total
 
Descriptive Properties
Content0.5Vulcanized Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH187 / 315105

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.