MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller TS820 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Low-Odor Structural Adhesive TS820 is a two-part, 1:1 mix ratio, toughened adhesive with less odor than most acrylic adhesives. TS820 Adhesive has excellent shear and peel strength along with good impact resistance and durability. TS820 Adhesive quickly bonds most metals and ceramics with minimal surface preparation.

Features and Benefits:

  • Low odor Acrylic Adhesive
  • Strong and durable adhesion
  • Minimal surface preparation
  • 1:1 mix ratio
  • Excellent shear and peel strength
  • High bond strength to stainless steel and galvanized steel

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 120000 - 160000 cP120000 - 160000 cPActivator, RV7 20 rpm
 240000 - 290000 cP240000 - 290000 cPResin, RV7 20 rpm
Storage Temperature -13.3 - -3.89 °C8.00 - 25.0 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 23.5 MPa3410 psiOver Lap, Cohesive Failure, Aluminum
 23.8 MPa3450 psiOver Lap, Cohesive Failure, Galvanized Steel
 24.5 MPa3550 psiOver Lap, Cohesive Failure, Stainless Steel
 25.8 MPa3740 psiOver Lap, Cohesive Failure, Carbon Steel
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourOpen Time
 15.0 min0.250 hourFixture Time
 1440 min24.0 hour
 
Descriptive Properties
ColorBlue
ConsistencyViscous Liquid
Mix Ratio1:1Volume
 1:1Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL099 / 316890

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.