MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Dexflex 992 NH533 BLK Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex 992 NH533 BLK very high melt flow, low flexural modulus, thermoplastic elastomeric olefin (TPO) has an excellent balance of properties. Applications: Automotive Parts, Exterior Automotive Applications.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 230 °C
32 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 500 %>= 500 %ISO 527-1,-2
Flexural Modulus 0.500 GPa72.5 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C131 °Funannealed; ISO 75B-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Dexflex 992 NH696 BLK Thermoplastic Polyolefin
Borealis Fibremod™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Asahi Kasei Thermylene® P6-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Polypropylene
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Polypropylene

PEQT7128 / 218765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.