MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48
Categories: Metal; Ferrous Metal; Cast Iron; Alloy Cast Iron; Gray Cast Iron

Material Notes: Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.

It often is used as an alternative to gray iron castings. The continuous casting process eliminates typical foundry defects, such as gas holes, hard spots, slag inclusions and inconsistent properties, that result from different molding methods.

Bars are cast through a water-cooled graphite die mounted on the bottom of a large bar machine crucible. The ferrostatic head pressure created by the molten metal in the bar machine crucible forces iron into the die, producing a very fine-grained microstructure. The outer “rim” is the only part of the bar that is solid when it exits the die. The core is molten iron. Heat from the molten iron core reheats the rapidly chilled outer skin, producing a homogenized microstructure that is cooled to room temperature in still air.

Gray iron bar stock’s microstructure consists of graphite flakes in a solid metal matrix. The solid metal matrix, in the class 40 grades (Dura-Bar grade G2), is pearlite.

The flake graphite provides excellent vibration damping for gears and machine tool components. Textile plant machinery utilize a lot of gray cast iron, because the damping coefficient reduces the factory noise The same holds true for machine tool components and automotive gears.

Compared to ductile iron, which has strengths closer to carbon steel, gray iron is the weaker, more brittle member of the cast iron family. Dura-Bar G2 is still considered an engineered material, having properties that are more than suitable for a wide variety of applications.

Composition: Typical chemical composition and ranges, actual values depend on cross section size.

Information provided by Dura-Bar.

Key Words: gray iron, class 40
Vendors: Dura-Bar Metal Services is the leading supplier of Dura-Bar® continuous cast iron and a major distributor of bronze alloys. Our customers rely on us for high quality materials that help increase their profitability. Call us at 1-800-526-0548 or visit dura-barms.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.06 - 7.34 g/cc0.255 - 0.265 lb/in³Approximately 10% lighter than carbon steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180 - 302180 - 302Depends on cast section size and location of test
Tensile Strength, Ultimate 276 MPa40000 psiTypical
Elongation at Break 1.0 %1.0 %Typical
Reduction of Area 2.0 %2.0 %
Tensile Modulus 124 GPa18000 ksiTypical
Compressive Yield Strength >= 827 MPa>= 120000 psiCompressive yield = compressive ultimate, approx 3X tensile strength
Compressive Strength >= 827 MPa>= 120000 psiCompressive yield = compressive ultimate, approx 3X tensile
Fatigue Strength 138 MPa
@# of Cycles 1.00e+8
20000 psi
@# of Cycles 1.00e+8
rotating beam
Shear Strength 400 MPa58000 psiShear strength will be 1.2 X tensile strength
Charpy Impact 6.78 J5.00 ft-lbGray iron usually not recommended in high impact loading applications
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.000011 ohm-cm0.000011 ohm-cmAt 2.50% Silicon
Magnetic Permeability 100 - 150100 - 15025 Oersted, High hysteresis loss
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.00 µm/m-°C
@Temperature 21.0 - 100 °C
5.00 µin/in-°F
@Temperature 69.8 - 212 °F
Mean
 9.50 µm/m-°C
@Temperature 21.0 - 300 °C
5.28 µin/in-°F
@Temperature 69.8 - 572 °F
Mean
 10.0 µm/m-°C
@Temperature 21.0 - 500 °C
5.56 µin/in-°F
@Temperature 69.8 - 932 °F
Mean
 11.0 µm/m-°C
@Temperature 21.0 - 900 °C
6.11 µin/in-°F
@Temperature 69.8 - 1650 °F
Mean
Specific Heat Capacity 0.506 J/g-°C0.121 BTU/lb-°F
Thermal Conductivity 53.329 W/m-K370.08 BTU-in/hr-ft²-°F
Melting Point 1120 °C2050 °FEutectic temp
Maximum Service Temperature, Air 649 °C1200 °FBrittle behavior throughout temperature range
Minimum Service Temperature, Air -59.4 °C-75.0 °F
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 0.020 - 0.20 %0.020 - 0.20 %
Carbon, C 2.7 - 4.0 %2.7 - 4.0 %
Chromium, Cr <= 0.050 %<= 0.050 %
Copper, Cu 0.050 - 0.30 %0.050 - 0.30 %
Iron, Fe 95 %95 %
Manganese, Mn 0.60 - 0.95 %0.60 - 0.95 %
Phosphorus, P 0.050 - 0.20 %0.050 - 0.20 %
Silicon, Si 1.8 - 3.0 %1.8 - 3.0 %
Sulfur, S 0.030 - 0.070 %0.030 - 0.070 %
Tin, Sn 0.10 - 0.30 %0.10 - 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
Dura-Bar G1 Continuously Cast Gray Iron Bar Stock ASTM A48
Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48
Overview of materials for Gray Cast Iron
Dura-Bar G1A Continuously Cast Gray Iron Bar Stock ASTM A48

NDURA05 / 16125

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.