MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Saint-Gobain COHRlastic® CF1877 Thermally Conductive Silicone Coated Fabric
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Conductive silicones expand the use of our products into the electronic assembly market. By the use of special fillers, silicone can be made thermally or electrically conductive. CF1877 is a thermally-conductive coated fabric providing thin, cost-effective heat transfer capability. It is obtainable plain or with thermally-conductive pressure sensitive adhesive on one side. All data based on a 0.0075 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength, Yield 89.6 MPa13000 psiASTM D412
Elongation at Break <= 5.0 %<= 5.0 %ASTM D412
Tear Strength 17.5 kN/m100 pliInitial Tear Strength; ASTM D624, Die B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D991
Dielectric Strength 15.7 kV/mm400 kV/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.25 W/m-K8.68 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorLight Green
Thermal Impedance (°Cin^2/W)0.24ASTM E1530

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® CF1869 Thermally Conductive Silicone Coated Fabric

PSTGQZ270 / 68784

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.