MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Primex Plastics Prime Impax 250 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Prime Impax 250 is a formulated High Impact Polystyrene that provides quality toughness, stiffness and impact strength. Prime Impax 250 is designed to meet a wide variety of product applications and is one of the most versatile, inexpensive materials we supply. It is our standard thermoforming grade of High Impact Polystyrene.

Applications: Prime Impax 250 is FDA compliant and USP Class VI compliant. With its ease of processing, it provides trays with the rigidity and parallelism need for good sealing. It is able to withstand Gamma Radiation and ETO sterilization.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Flow 2.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75ASTM D785
Tensile Strength, Yield 2900 psiASTM D638
Elongation at Break 70 %ASTM D638
Flexural Modulus 275000 psiASTM D790
Izod Impact, Notched 2.10 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 183 °FASTM D648
Vicat Softening Point 210 °FASTM D1525
Flammability, UL94 HB
@Thickness >=1.52 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRIM023 / 278494

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.