MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Dow™ DGDC-2100 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DGDC-2100 NT 7 HDPE resin is a high-molecular weight, high density film grade resin. This product was specifically designed to offer an optimal balance of physical properties and processability. DGDC-2100 NT 7 HDPE resin is ideally suited for use in making grocery sacks, consumer and institutional liners, and merchandise bags.
Complies with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU, No 10/2011. Consult the regulations for complete details.

Availability: Asia Pacific; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520© 3.2; HPFB (Canada) No Objection; EU, No 10/2011

Form: Pellets

Processing Method: Blown Film; Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Melt Flow 0.070 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 6.70 lb (f)
@Thickness 0.0127 mm
Film Tensile Strength at Yield, MD 6140 psi
@Thickness 0.0127 mm
ASTM D882
Film Tensile Strength at Yield, TD 4610 psi
@Thickness 0.0127 mm
ASTM D882
Film Elongation at Break, MD 330 %
@Thickness 0.0127 mm
ASTM D882
Film Elongation at Break, TD 410 %
@Thickness 0.0127 mm
ASTM D882
2% Secant Modulus 140000 psi
@Thickness 0.0127 mm
MD; ASTM D882
 159000 psi
@Thickness 0.0127 mm
TD; ASTM D882
Puncture Energy 7.90 in-lb
@Thickness 0.0127 mm
Elmendorf Tear Strength MD 11 gASTM D1922
Elmendorf Tear Strength TD 73 g0.0005; ASTM D1922
Dart Drop Test 350 g
@Thickness 0.0127 mm
ASTM D1709A
Film Tensile Strength at Break, MD 13600 psi
@Thickness 0.0127 mm
ASTM D882
Film Tensile Strength at Break, TD 9990 psi
@Thickness 0.0127 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °F
 
Optical PropertiesOriginal ValueComments
Haze 69 %
@Thickness 0.0127 mm
ASTM D1003
Gloss 9.0 %
@Thickness 0.0127 mm
45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 410 °FExtrusion
Blow-up Ratio (BUR) 4.0
 
Descriptive Properties
Film Puncture Resistance128 ft-lb/in30.5 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF440 / 311133

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.