MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical Goyenchem-GPPS23 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Characteristic:
  • Injection Grade
  • Low Residual Monomer
  • Good Heat Resistance
  • Mold Dimension Stability
  • Excellent Transparency
  • Easy Processing
  • Good Electrical Properties
Applications:
  • Stationery, rulers, thumbtacks, petri-dishes, alarm clocks.
  • Cosmetic cases, spray bottles, Christmas lights, toys, home applications.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123ASTM D785
Tensile Strength, Yield 44.1 MPa
@Thickness 3.17 mm
6400 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 2.0 %
@Thickness 3.17 mm
2.0 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 71.6 MPa
@Load 1.00 kg,
Thickness 3.00 mm
10400 psi
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D790
Flexural Modulus 3.53 GPa
@Load 1.00 kg,
Thickness 3.00 mm
512 ksi
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D790
Izod Impact, Notched 0.137 J/cm0.257 ft-lb/inA method, 1/4”×1/2”×5/2”; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 12.7 mm
194 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 100 °C
@Load 1.00 kg,
Thickness 3.00 mm
212 °F
@Load 2.20 lb,
Thickness 0.118 in
120°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.40 %
@Thickness 2.80 mm
0.40 %
@Thickness 0.110 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 280 °C320 - 536 °FCylinder
Mold Temperature 35.0 - 65.0 °C95.0 - 149 °F
Injection Pressure 49.0 - 137 MPa7110 - 19900 psi
 
Descriptive Properties
Composition200 ppmResidual SM monomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN789 / 267097

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.