MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ConocoPhillips Hydroclear® 100 Turbine Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formulated with proprietary additive chemistry to meet the requirements of steam, gas and hydroelectric turbine service. Hydroclear Turbine Oil also can be used successfully in pumps, motors and a variety of other industrial applications where a premium rust- and oxidation-inhibited oil is recommended. Hydroclear Turbine Oil has been tested and formally approved by Cincinnati Milacron under specifications P-38 (ISO 32), P-55 (46) and P-54 (68).

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.872 g/cc0.0315 lb/in³
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 510 SUS510 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 98 cSt98 cSt
Kinematic Viscosity at 100°C (212°F) 11.3 cSt11.3 cSt
Oxidative Stability 7500 hour7500 hourASTM D 943
ASTM Color 0.500.50
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 30.0 kV/mm>= 762 kV/inNo thickness given; ASTM D877
 
Thermal PropertiesMetricEnglishComments
Pour Point -28.9 °C-20.0 °F
Rotating Bomb Oxidation Test (RBOT) 850 min850 minASTM D 2272
Flash Point 254 °C490 °F
 
Descriptive Properties
Emulsion Characteristics (40-40-0)10 minutes
ZincMax 10 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON133 / 75170

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.