MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound RC003 Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP THERMOCOMP RC003 compound is based on Nylon 6/6 resin containing 15% carbon fiber. Added features of this grade include: Electrically Conductive.

Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %Injection Molding
Water Absorption at Saturation 5.5 %5.5 %ISO 62-1
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 105105ISO 2039-2
Tensile Strength at Break 170 MPa24700 psi5 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 13.0 GPa1890 ksi1 mm/min; ISO 527
Flexural Strength 230 MPa33400 psibreak, 2mm/min; ISO 178
Flexural Modulus 10.0 GPa1450 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
80*10*4; ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 178000 ohm-cm178000 ohm-cmIEC 60093
Surface Resistance 178000 ohm178000 ohmROA; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
11.1 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 252 °C486 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 255 °C491 °FRate B/120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
UL 94 by SABIC-IP
Oxygen Index 28 %28 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 250 - 270 °C482 - 518 °F
Zone 2 260 - 280 °C500 - 536 °F
Zone 3 260 - 280 °C500 - 536 °F
Melt Temperature 260 - 290 °C500 - 554 °FInjection Molding
Mold Temperature 70.0 - 120 °C158 - 248 °F
Drying Temperature 75.0 - 85.0 °C167 - 185 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81823 / 289770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.