MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 526N High Performance Epoxide
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Clear-Amber, 1:1 System for Tough Bonding Applications
Also available filled with aluminum oxide (Alumina) or pigments

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/cc
Viscosity 8500 cP8500 cPMixed Viscosity
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989
Flexural Strength 124 MPa18000 psiASTM D790
Shear Strength 19.3 MPa2800 psiASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+14 ohm-cm4.00e+14 ohm-cm
Dielectric Constant 3.01
@Frequency 1000 Hz
3.01
@Frequency 1000 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
Dissipation Factor 0.0100.010
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.4 µm/m-°C
@Temperature 20.0 °C
18.0 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 300 °C572 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min4.00 hour2 hrs at 200°F; 2 hrs at 325°F (Recommended Cure)
 180 - 240 min
@Temperature 149 °C
3.00 - 4.00 hour
@Temperature 300 °F
Alternate Cure
Pot Life 150 min
@Temperature 25.0 °C
150 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceGood
ColorAmber
Mix Ratio by Weight1:1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Raschig Group EPOXIDUR® 3580 EP Epoxy
Aremco Aremco-Bond™ 2318 High Performance Epoxide
Hexcel® HexPly® F593 Epoxy Resin
Overview of materials for Epoxy Adhesive

PAREM00 / 24264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.