Product description: VINNAPAS® 7016 F is a plasticizing dispersible polymer powder based on vinyl acetate, ethylene and methyl methacrylate with instant plasticizing effect, casein-like rheology and very good self-healing effect especially for manually applied systems. Properties: VINNAPAS® 7016 F is a terpolymer powder of vinyl acetate, ethylene and acrylate. It is dispersible in water and is also a highly effective plasticizing admixture with rheological properties similar to those of casein. VINNAPAS® 7016 F is ideal for formulating cementitious and gypsum-based flooring systems (e.g. self-leveling flooring compounds). Thereby the rheology of VINNAPAS® 7016 F is especially advantageous for the manual application. VINNAPAS® 7016 F contains a fine mineral filler as an antiblocking agent and is produced without the addition of organic solvents, plasticizers and film-forming agents. Special features: VINNAPAS® 7016 F is a high-quality hard polymeric binder and is also a highly effective plasticizing admixture with casein-like rheology. There is no need to add any commercial plasticizing admixtures when 2- 3 % VINNAPAS® 7016 F is added to a blend. VINNAPAS® 7016 F is especially suitable for the formulation of self-leveling flooring compounds with low emissions. Information provided by Wacker Chemie AG. |